Graphical Abstract
|
Highlights
- Optimization of SLM process parameters ensures the production of high-quality, mechanically robust maraging 300 alloy parts.
- Optimal energy density minimizes porosity and unmelted particles, resulting in improved density and strength.
- Heat treatment significantly enhances tensile strength through solution and aging processes.
- The stripe scanning strategy improves tensile strength and reduces porosity compared to alternative strategies.